Good evening
I cannot for the life of me remember how one could calculate shear capacity of an alluminium beam (used for formwork/falsework applications) and it's embarressing. Given the following information, can someone put me out of my misery?
Cross sectional area, = 3000 mm2
E = 69000 MPa
Mom of intertia, (Ixx) = 21.0 x 10^6 mm^4
Shear rigidity (GAxx) = 35110 kN
Section Modulus (Zxx) = 189 x 10^3 mm^3
Radii of Gyration (ryy) = 29.8 mm
Edit: I am not a Structural engineer although I did train to be (college).
Thank you
I cannot for the life of me remember how one could calculate shear capacity of an alluminium beam (used for formwork/falsework applications) and it's embarressing. Given the following information, can someone put me out of my misery?
Cross sectional area, = 3000 mm2
E = 69000 MPa
Mom of intertia, (Ixx) = 21.0 x 10^6 mm^4
Shear rigidity (GAxx) = 35110 kN
Section Modulus (Zxx) = 189 x 10^3 mm^3
Radii of Gyration (ryy) = 29.8 mm
Edit: I am not a Structural engineer although I did train to be (college).
Thank you