Base Plate Grout

Status
Not open for further replies.

nbryan

Civil/Environmental
Apr 25, 2001
18
Is there a test method or an acceptable practice for testing
base plate grout in the field?
 
Replies continue below

Recommended for you

Suggest you make cubes of the grout and match cure them alongside the base. Then crush them at the times you require to test the strength. If you have already cast the grout then the best I can suggest is a re-batch using the same mix design and test sufficient numbers of cubes until you and your client are satisfied that statistically you are covered for strength. Andy Machon


 