Today I was reviewing WPS and PQR submitted by our subcontractor.
PQR was made on a pipe NPS 18 with 11.13 nominal wall thickness, this info comes from MTR. But on PQR base metal thickness is recorded to be 9.6 mm. What I guess, he deducted 12.5% allowance on the wall thickness.
In my opinion base metal thickness should be nominal thickness, am I correct?
Secondly if 9.6 mm is the thickness of coupon, PQR shows 4 side bend tests while QW-451 permits 4 side bends if thickness is 10 mm and over. May the difference of just 0.4 mm (10-9.6 = 0.4 mm) be tolerated and side bends be accepted? in lieu of two root, two face bends?
Nasir
Welding Engineer
DESCON ENGINEERING LIMITED
PAKISTAN
PQR was made on a pipe NPS 18 with 11.13 nominal wall thickness, this info comes from MTR. But on PQR base metal thickness is recorded to be 9.6 mm. What I guess, he deducted 12.5% allowance on the wall thickness.
In my opinion base metal thickness should be nominal thickness, am I correct?
Secondly if 9.6 mm is the thickness of coupon, PQR shows 4 side bend tests while QW-451 permits 4 side bends if thickness is 10 mm and over. May the difference of just 0.4 mm (10-9.6 = 0.4 mm) be tolerated and side bends be accepted? in lieu of two root, two face bends?
Nasir
Welding Engineer
DESCON ENGINEERING LIMITED
PAKISTAN