Dear Friends
I want guidance in qualifying PQR
Applicable Code AWSD1.1.
6GR Test Position- API 5L X52 Pipe used( Group II- Impact Test Reqd.)
Question -
1) Is it mandatory to do mock-up test?
2) Is there any base material limitations for preparing macro specimen.
Thanks
 