Based on visual inspection how can I classify the bedrock on a riverbed if it is Gabbro or Basalt?
 
Replies continue below

Recommended for you

color and grain size?
 
Gabbro is coarser grained - almost like granite. Basalt is uniformly dark gray or black and fine grained. Here's a chart on igneous rocks:

ignrxclass.gif


f-d

¡papá gordo ain’t no madre flaca!
 
basalt gray or black
gabro more green
 
fattdad your the best..Thank you for the information..
 