Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Barites concrete - properties

Status
Not open for further replies.

bkal

Structural
Feb 27, 2003
272
Hello,

we were asked to look into using barites concrete for some shielding walls. I am a bit concerned abut its shrinkage and thermal properties, but cannot find any reference regarding how does it comapre with 'normal' concrete. I would appreciate any information in this respect.

Thanks in advance.
 
Replies continue below

Recommended for you

have used Barite aggregate for nuclear shielding and other than it being very heavy, had no difficulty with the use of it. You may want to talk to a concrete supplier.

Dik
 
Due to the potential for segregation during placement, make sure the slump is kept low.
 
Thanks for helping with this. Shrinkage is important in this case as heavyweight concrete elements are mixed (joined to) standard concrete. Due to the nature of the facility, these elements need to provide containement, so any cracking needs to be minimised.
 