Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Backing material for Al6061 MIG

Status
Not open for further replies.

IFRs

Petroleum
Nov 22, 2002
4,674
I have tried using a copper block as a removable backing for welding 0.18 inch thick AL6061 using 4043 MIG but the copper block is sticking to the weld. Would carbon steel stainless steel, graphite, etc be the best choice? This is used inside a channel shape, the channels are legs towards each other in a 90 degree corner, we are welding the 45 degree mitered flanges and vertical web. Thanks!
 