Fizza453
Mechanical
- Jun 22, 2011
- 262
While making full penetration groove welds in SS with GTAW, we use back purging at root.
I came to know that there is such a wire exists that does not require back purging, is there such a wire? its name? its manufacturer?
Nasir
Welding Engineer
DESCON ENGINEERING LIMITED
PAKISTAN
I came to know that there is such a wire exists that does not require back purging, is there such a wire? its name? its manufacturer?
Nasir
Welding Engineer
DESCON ENGINEERING LIMITED
PAKISTAN