Trying to design a piping system with duplex pipe material S31803 A928 CL1 to ASME B31.3.
B31.3 does not list the stress values for this material.
Is the correct procedure to use a similar material in B31.3, say A790 S31803 or should one refer to ASME II Part D?
Per the example above if one compares the stress value at say 200°C, then the
A928 S31803 = A240 = 165MPA (from Part D)
A790 S31803 = 198.7MPA (from B31.3)
Any advice much appreciated.