Im doing some calcs for a thermowell at high pressure and temperature. Material is UNS N06600 at 550 °C design. Using para 304.1.3, I run into the issue that I cant determine Pa2 since (b) requires me to calculate 90% of yield for N06600 acc. ASME II-D table Y-1. Table Y-1 ends at 500 °C for N06600 (or at 525 °C for certain ASTM specs). I believe some time ago this question was asked here as well, but I cant remember the outcome. Any ideas?