In the 2014 edition of B31.3, Para 331.1.7 was removed as well as the BHN values in Table 331.1.1. However, Para 331.1.7 is still referenced throughout the standard.
Does this mean that Hardness testing is no longer required after PWHT?
Mohammed Diab.
Inspection Supervisor - Saudi Aramco.
Does this mean that Hardness testing is no longer required after PWHT?
Mohammed Diab.