I am currently working on a wellhead system, to API 6A and B31.3 Chapter IX High Pressure Piping, my question is to calculate the thickness of an inline 2’’ NB Blind, I was using Para K304.5.3 Blanks(B31.3), which stipulates Allowable Stress from Table K-1. However the Material is Alloy 625 UNS N06625 which is not represented in Table K-1. Would I be correct in referring to Table A-1 where the Material is available.
Thanks in advance