If a nozzle is to be welded to a standard pipe cap, should the pipe cap now be calculated as a 2:1 elliptical head instead of straight pipe since it is being modified from its original form?
 
Replies continue below

Recommended for you

Yes I believe so as there is no allowance for cuting holes and welding to fittings in B16.9 as far as a I can see, unlike e.g. a blind flange.

Remember - More details = better answers
Also: If you get a response it's polite to respond to it.
 
You need to calculate the required nozzle neck thickness and the reinforcement (ASME VIII-1 UG-45 and UG-37)