Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

B-H-curves

Status
Not open for further replies.

marcoabelius

Mechanical
Joined
Feb 4, 2005
Messages
4
Location
DE
I'm looking for a B-H-curve of the stainless steel 1.4104 (AISI 430 F). Does anyone know where I can find it on the internet?
 

However, this will give the flux density up to magnetizing force of 100 Orsteds.

You may need to go through the registration process to reach this page.

A better B-H graph you should find in ASM metals handbooks which will give the flux density up to very high magnetizing force (saturaion).
 
CARPENTER TYPE 430
ANNEALED (75.5 HRB)
1450F 2 hours dry H2

H (Oe) B (Gauss)
0.00 0.00
0.39 85.05
0.92 340.21
1.45 595.36
1.71 850.52
2.11 1275.77
2.24 1615.98
2.37 2041.24
2.50 2466.49
2.63 2891.75
2.89 3487.11
3.03 4167.53
3.16 4762.89
3.29 5188.14
3.42 5783.51
3.55 6463.92
3.68 7144.33
3.95 7824.74
4.21 8420.10
4.47 8930.41
4.74 9355.67
5.00 9865.98
5.39 10376.30
5.79 10886.60
6.18 11226.80
7.11 11652.10
7.76 11907.20
9.08 12332.50
10.26 12502.60
11.45 12757.70
13.16 12927.80
14.74 13012.90
16.32 13183.00
17.89 13268.00
19.08 13353.10
22.24 13523.20
23.95 13608.20
25.39 13693.30
26.58 13693.30
27.89 13778.40
28.82 13778.40
29.87 13778.40
31.58 13706.30
39.47 13881.00
46.05 14055.60
57.89 14317.50
69.74 14579.40
82.89 14841.30
97.37 15015.90
114.47 15277.80
128.95 15452.40
142.11 15539.70
157.90 15714.30
175.00 15888.90
190.79 15976.20
206.58 16063.50
227.63 16150.80
246.05 16238.10
264.47 16325.40
282.90 16412.70
300.00 16412.70
 