May 14, 2008 #1 VRuiz Marine/Ocean Joined Apr 24, 2008 Messages 4 Location ES Please, I need to know the B-H (Flux density - field intensity) curve for "Steel F-111" Where can I find it? Could anybody send it to me? Thank you
Please, I need to know the B-H (Flux density - field intensity) curve for "Steel F-111" Where can I find it? Could anybody send it to me? Thank you
May 15, 2008 Thread starter #2 VRuiz Marine/Ocean Joined Apr 24, 2008 Messages 4 Location ES I'm sorry, I realized "F-111" is in IHA designation, the equivalent for: UNE "F-1110" DIN "C15(CK15)" ASTM "1015" NF "XC12" BS "EN.2" Thank you Upvote 0 Downvote
I'm sorry, I realized "F-111" is in IHA designation, the equivalent for: UNE "F-1110" DIN "C15(CK15)" ASTM "1015" NF "XC12" BS "EN.2" Thank you