Does anybody know where to find the B-H curve for Duplex UNS s32001 (Nitronic 19D by AK Steel)? I tried the website of AK Steel but no luck.
 
Replies continue below

Recommended for you

call AK tech support and ask.
In general these alloys are not really all that magnetic. They are only half ferrite so saturation will be less than 10k, more like 7k probably. No idea about initial perm or coercive.

= = = = = = = = = = = = = = = = = = = =
Plymouth Tube
 
Status