Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations TugboatEng on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

B-H Curve for 12L14 Carbon Steel 1

Status
Not open for further replies.

avocadozo

Aerospace
Joined
Jun 29, 2005
Messages
8
Location
US
I want to get the B-H curve for 12L14 Carbon Steel. Is there anyone to know the information about the B-H curve?
 
You can use the AISI 1020, 1018, 1010 instead. The differences are minor. You can find B-H for AISI 1010 at the ASM METALS HANDBOOK 8th editiom.
 
I meant use the B-H curves of AISI 1020, 1018, 1010 instead.
 
I found an old photocopy of an article from a trade magazine that has a bunch of curves, including one for 12L14. I extracted some points from it:
H(Oe) B(Gauss)
1 500
2 3500
3 5800
4 7700
5 9300
6 10000
7 10600
10 12000
20 14000
30 15000
70 16300

Please keep in mind, these are only approximate values.