Hello All: I came from a Mil-278 background and my new job is asking about getting compliant with section IX for CRN Registration purposes. A few questions. As I read the code it does not appear to address joint design, base metals, inspections or welder training?? Are the requirements of B31.1 and B31.3 incorporated under Section IX. Do they allow Autogenous welds?? Mil-278 did not. Our alloys are 304 tube to 430 FR bar with no specifications assigned to them, yet. Is that OK ?