Hi All,
I would like to know the minimum depth of partial joint penetration that is pre-qualified by AWS D1.6 for the following AISI Type 316 standard pipe sections:
3" pipe
4" pipe
8" pipe
I don't have the AWS D1.6 code (nor the AWS D1.1) to use as a reference or compare. A pair of 8" pipes are used as structural columnns, 25 ft high, braced together with the 3" and 4" diameter pipes as to support an aerobic mixer platform in an oxidation ditch (wastewater plant). Thanks for your assistance.
I would like to know the minimum depth of partial joint penetration that is pre-qualified by AWS D1.6 for the following AISI Type 316 standard pipe sections:
3" pipe
4" pipe
8" pipe
I don't have the AWS D1.6 code (nor the AWS D1.1) to use as a reference or compare. A pair of 8" pipes are used as structural columnns, 25 ft high, braced together with the 3" and 4" diameter pipes as to support an aerobic mixer platform in an oxidation ditch (wastewater plant). Thanks for your assistance.