FredTechWelding
Petroleum
Dear all,
A multiple process weld is performed on one of my projects. Applicable standard is AWS D1.1.
Starting with GTAW for the root and 1st layers and then filling and capping with SAW.
My question is : May it be possible to qualify one welder for both processes at the same time ?
The expected welder qualification will be practiced according to the WPS used for this weld (same processes, same sequence, same dimensions (diameter & thickness), same positions.
This welder qualification will only be used for the specific weld described above.
Welder qualification tests will be practiced according to AWS requirements.
The welder who performed the weld qualification (WPQR) is qualified but we want to qualify one additional welder.
The AWS D1.1 does no mention anything concerning the welder qualification for multiple process weld. Is this meaning that this practice is not allowed ?
Thanks in advance for your help
A multiple process weld is performed on one of my projects. Applicable standard is AWS D1.1.
Starting with GTAW for the root and 1st layers and then filling and capping with SAW.
My question is : May it be possible to qualify one welder for both processes at the same time ?
The expected welder qualification will be practiced according to the WPS used for this weld (same processes, same sequence, same dimensions (diameter & thickness), same positions.
This welder qualification will only be used for the specific weld described above.
Welder qualification tests will be practiced according to AWS requirements.
The welder who performed the weld qualification (WPQR) is qualified but we want to qualify one additional welder.
The AWS D1.1 does no mention anything concerning the welder qualification for multiple process weld. Is this meaning that this practice is not allowed ?
Thanks in advance for your help