I am reviewing a welding procedure PQR. It is for a plate welded in 2G position, but the actual part is a bellows circumferential weld to machined components on either end. it is likely to be a rolling 2G instead. Does a 2G qualify a rolling 2G?
 
Replies continue below

Recommended for you

If we are thinking about the same thing, it is typically designated as 1G-R, as the weld puddle is very near the top of the part. Also, watch out for which side of top-dead-center the puddle is on - a lot of times GMAW/MAG is done 1G-R downhill.

Thus the answer is yes, the 2G coupon is adequate.
 
kevlar,
"Does a 2G qualify a rolling 2G?"

Did you actually mean "Does a 2G qualify a rolling 1G ?"

Cheers,
DD
 