Is a “ENG-TIPS” posting from 8April2004 not currently(1June2011) correct in that the upper limits of C & Mn have since been defined for JIS SS400?
The weblink address for this thread posting is :
I don’t have access to any complete JIS publications but I have uploaded the attached PDF with some specs for JIS SS400 & ASTM A36 are from a google search on 31May2011:
Per the attached PDF , the allowable limits are - Cmax is 0.22% and Mn max is 0.6%
Thanks in advance for feedback on this (especially if it is given before 4June2011...so I can make an assesment before my due date regarding this issue)!