May 2, 2013 #1 kdizzle Structural Joined May 2, 2013 Messages 1 Location US I have 2.875od x2.125id. grade 1026-AK A-513 type 5 how can you tell group number(1-5)it is in the AWS D1.1 2010 book? Its not listed in any groups.
I have 2.875od x2.125id. grade 1026-AK A-513 type 5 how can you tell group number(1-5)it is in the AWS D1.1 2010 book? Its not listed in any groups.
May 3, 2013 #2 Mr168 Materials Joined Aug 5, 2008 Messages 731 Location US Unlisted materials are not assigned a group number, and consequently may not be welded using a prequalified WPS. The WPS must be qualified in accordance with Clause 4. Upvote 0 Downvote
Unlisted materials are not assigned a group number, and consequently may not be welded using a prequalified WPS. The WPS must be qualified in accordance with Clause 4.