NEED HELP TO FIND THIS MATERIAL (ZERON 100)IN US.IT IS AVAILABLE IN U.K., BUT EXPENSIVE TO BRINGING IN US.SHOP QUOTING AGAINST US BUYING IN US, BUT WE CAN NOT LOCATE A VENDER.THANKS IN ADVANCE.
I believe that Allegheny Ludlum is making some limited product forms under lic..
Expensive does not begin to describe superduplexs. The alloys are expensive to start with, and a bear to process.
= = = = = = = = = = = = = = = = = = = =
Rust never sleeps
Neither should your protection