Can anyone recommend a good source for information on autoclave steam curing of rolls of calendered rubber sheeting? I'm mostly interested in trouble shooting of defects such as blisters, voids, etc. Any guidance would be appreciated.
 
Replies continue below

Recommended for you

Te recomiendo "How to improve rubber compounds" de John S. Dick.
 