mmitpwdba
Industrial
- May 31, 2002
- 6
Need some material suggestions for an atomizer that changes a liquid into a powder for the food industry.
Current material is a 400 series stainless heat treated to 55-60 Rc.
This is a multiple part assembly that is experiencing extremely abrasive wear.
Machinability is also a concern.
Any help would be greatly appreciated.
Thanks,
Jeff
Current material is a 400 series stainless heat treated to 55-60 Rc.
This is a multiple part assembly that is experiencing extremely abrasive wear.
Machinability is also a concern.
Any help would be greatly appreciated.
Thanks,
Jeff