Can anyone share material spec for M20 & M30 washers. I have a situation where I get deviation from the vendor to ASTM F436M for M20 & M30 washers..however i do not have the basis to chack if this is acceptable or not.Below is snapshot of the material certificate.
Capture_nbfu7k.png
 
What does the vendor's deviation request state? If they can't identify the deviation they are pretty worthless as a vendor.

FWIW, that spec calls for material with a certain amount of Ni, Cr and Cu...which apparently were not found or not included in the analysis.
 