Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

ASTM Equivalency for 1144 Straight

Status
Not open for further replies.

brakemeister

Automotive
Aug 15, 2002
41
Can anyone tell me if there is an ASTM standard that is equivalent to AISI 1144 Straight (not Stressproof and not stress-relieved).
 
Replies continue below

Recommended for you

First, AISI no longer maintains standards for steel chemical composition, so there is no such thing as AISI 1144. The grade 1144 appears in a number of standards, such as the following:

SAE J403 - Chemical composition only
SAE J935 - High strength die-drawn bar standard, with 1144 being one of the grades
ASTM A 29 - Hot rolled bar standard, with 1144 being one of the grades
ASTM A 108 - Cold drawn bar standard, with 1144 being one of the grades

The choice of ASTM standard depends on the product form (cold-drawn bar, hot-rolled wire rod, etc.) that is required.
 