I'm looking to use ASTM D4000-12 or ASTM D4066-01 on some engineering drawings. I have determined that I need the following:
ASTM D4066-01 PA 011 B0003___ <--This 5th line item is "to be determined" and I'd like to use this position to add in a brittleness temp/cold temp application requirement but I do not know how to use that "to be determined" slot. (See page 9 in the standard).
I also am looking to make sure I understand both standards as I think both are applicable to my application, so I believe that the callout below equals the same.
ASTM D4000-12 PA 011 E0004___ <-- Here I would also like to use the "to be determined" for the brittleness temp.
Any advice on this would be greatly appreciated!
Thank you!
I'm looking to use ASTM D4000-12 or ASTM D4066-01 on some engineering drawings. I have determined that I need the following:
ASTM D4066-01 PA 011 B0003___ <--This 5th line item is "to be determined" and I'd like to use this position to add in a brittleness temp/cold temp application requirement but I do not know how to use that "to be determined" slot. (See page 9 in the standard).
I also am looking to make sure I understand both standards as I think both are applicable to my application, so I believe that the callout below equals the same.
ASTM D4000-12 PA 011 E0004___ <-- Here I would also like to use the "to be determined" for the brittleness temp.
Any advice on this would be greatly appreciated!