Anyone know of an ASTM standard for a corrosion creepback test performed in salt spray? I am looking for something comparable to GM 9102P.
 
Replies continue below

Recommended for you

ASTM D1654-05 Standard Test Method for Evaluation of Painted or Coated Specimens Subjected to Corrosive Environments

Regards,

Cory

Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
Thanks, Cory. That is exactly what I was looking for. Unclesyd--I'm getting ready to evaluate some non phosphate pre-treatments for epoxy powder coat.
 