Oct 26, 2006 #1 swall Materials Joined Sep 30, 2003 Messages 2,767 Location US Anyone know of an ASTM standard for a corrosion creepback test performed in salt spray? I am looking for something comparable to GM 9102P.
Anyone know of an ASTM standard for a corrosion creepback test performed in salt spray? I am looking for something comparable to GM 9102P.
Oct 26, 2006 1 #2 CoryPad Materials Joined Apr 15, 2002 Messages 5,192 Location US ASTM D1654-05 Standard Test Method for Evaluation of Painted or Coated Specimens Subjected to Corrosive Environments Regards, Cory Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora. Upvote 0 Downvote
ASTM D1654-05 Standard Test Method for Evaluation of Painted or Coated Specimens Subjected to Corrosive Environments Regards, Cory Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
Oct 26, 2006 #3 unclesyd Materials Joined Aug 21, 2002 Messages 9,819 Location US What is your area area of concerned with coatings? There are tests for different areas. Here is the source of some KTA test panels. http://www.ktagage.com/level2.asp?category_ID=29 Upvote 0 Downvote
What is your area area of concerned with coatings? There are tests for different areas. Here is the source of some KTA test panels. http://www.ktagage.com/level2.asp?category_ID=29
Oct 27, 2006 Thread starter #4 swall Materials Joined Sep 30, 2003 Messages 2,767 Location US Thanks, Cory. That is exactly what I was looking for. Unclesyd--I'm getting ready to evaluate some non phosphate pre-treatments for epoxy powder coat. Upvote 0 Downvote
Thanks, Cory. That is exactly what I was looking for. Unclesyd--I'm getting ready to evaluate some non phosphate pre-treatments for epoxy powder coat.