Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations KootK on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

ASTM A995 6A DUPLEX, B16.34 Approved?

Status
Not open for further replies.

SmithDavid

Petroleum
Jul 8, 2009
2
I have a customer that's specified ASTM A995 6a for valves and designed per ASME B16.34.

I'm trying to confirm if this Cast version of Super Duplex is a recognized material in B16.34.



 
Replies continue below

Recommended for you

ASTM A995 6a is not listed in Table 1 of ASME B16.34-2004. Look at ASTM A351 instead for cast duplex stainless steel castings.
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor