No. The ASME SA 672 Specification is for "Electric-Fusion- Welded Steel Pipe for High Pressure Service at Moderate Temperatures".
The Grade C70 refers to ASTM A 516 Grade 70 plate for fabricating the welded steel pipe. This is plain carbon steel plate, killed, fine grained.