I have a question regarding the mechanical testing results for A536 70-50-05 material. I have a supplier who does both seperate and cast on samples however their acceptance criteria for cast on samples is significantly lower than what A536 specifies for 70-50-05. Where A536 calls for a tensile of 485 MPa and a yeild of 345 MPa the supplier accepts tensiles of 379 MPa and yeilds of 272 MPa for their cast on samples. If the cast on samples have significantly lower properties than are specified how can the material be considered 70-50-05 when the mechanical properties are what A536 bases its classifications on? Thanks in advance for your replies.