Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

ASTM A515 GR. 70 1

Status
Not open for further replies.

NAITSABES

Mechanical
Jun 26, 2007
2
Grettings everyone.
I would like to know if some can bring me some information about this material, mechanical properties, chemical composition and the kind of applications in vessel pressures.
Something like tha range of pressure, temperature and conditions, where I should use this plate steel material.

Thank you.
I will appreciate your help.
 
Replies continue below

Recommended for you

.........and the allowable pressure and temperature depend upon the diameter and wall thickness of your pressure vessel as that will affect the stress in the material (note the ASME Code allowable stresses). In addition, any openings in the vessel (and their reinforcement) MUST be designed by a MECHANICAL ENGINEER (and you do not sound like you are one).
 
A-515 Gr 70 has a 70 ksi to 90 ksi (485 MPa to 620 MPa)
ultimate tensile strength. The minimum yield strength is 38 ksi(260 MPa. Plates over 2" thick must be normalized. The steel shall be silicon killed (fully deoxidized) and made to coarse grain size practice.

A-515 is preferred for use at operating temperatures above 650 F. It is not recommended for use in low temperature applications.

 