Aug 25, 2004 #1 taregan Materials Joined Sep 20, 1999 Messages 8 Location US Looking for Young's modulus, Poisson's ratio and density of ASTM A401 steel.
Aug 25, 2004 #2 Carburize Materials Joined Sep 23, 2002 Messages 702 Location US 210 Gpa 0.29 7.85 g/cc Upvote 0 Downvote
Aug 26, 2004 #3 NickE Materials Joined Jan 14, 2003 Messages 1,570 Location US Good on Carburize! Upvote 0 Downvote
Aug 26, 2004 Thread starter #4 taregan Materials Joined Sep 20, 1999 Messages 8 Location US Thanks Carburize. What's your source for the data? Upvote 0 Downvote
Aug 26, 2004 #5 Carburize Materials Joined Sep 23, 2002 Messages 702 Location US I use "Smithells Metals Reference Book" Seventh Edition (ISBN 0-7506-3624-6) as my main source for this type of data. Upvote 0 Downvote
I use "Smithells Metals Reference Book" Seventh Edition (ISBN 0-7506-3624-6) as my main source for this type of data.