Looking for Young's modulus, Poisson's ratio and density of ASTM A401 steel.
 
Thanks Carburize. What's your source for the data?
 
I use "Smithells Metals Reference Book" Seventh Edition (ISBN 0-7506-3624-6) as my main source for this type of data.
 