Jadson

Mechanical
Mar 28, 2021
7
I'm trying to determine the wall thickness of a pipe that has a design pressure of 15,000 psi at 700 F.
The specified material is ASTM A335 P91. I have to use ASME B31.3 chapter IX (defined by the owner). The problem is that ASTM A 335 P91 is listed only in Appendix A. Can I use the allowable stress from Table A-1 in the equations to calculate the required wall thickness in paragraph K304.1.2 (chapter IX)?

Thanks in advance for your help.
 
Replies continue below

Recommended for you

See K302.2.2(b) "Piping components that do not have allowable stresses or P-T ratings shall be qualified for pressure design as required by K304.7.2"

----------------------------------
Not making a decision is a decision in itself
 
Short: no. For chapter IX, you need to use allowable stresses from table K-1.

Huub
- You never get what you expect, you only get what you inspect.
 
Thank you all very much for your answers. Therefore, as a conclusion, if I use ASTM A335 P91, I´ll have to calculate the allowable stress values at design temperature not exceed the lower of two-thirds of SY and two thirds of Syt. But I think there is a reason for ASME not to use ASTM A335 P91 in table K-1. Does anyone know why?
 
The reason why P91 may not be in table K-1; we don't know. At least I don't. Code committee consists of volunteers that together try to improve the code. Sometimes, they forget something, and sometimes, people don't ask for certain materials to become a code listed materials. What ever the reason, one may guess.

As for the 2/3 on yield; table K-1 has its own way to dervie the allowable stresses listed in table K-1; review K302.3.2.

Huub
- You never get what you expect, you only get what you inspect.
 