I'm struggling to find where the mechanical property requirements (tensile, hardness, elongation) are for T22 material. Properties are listed for some of the other grades in the A213 standard however.

Is this intentional? If so, are there any adopted standards as far as mechanical properties are concerned?

Thanks
 
Replies continue below

Recommended for you

No. I have A/SA 213 Specification, SA 213-08, the T11 and T22 are listed in Table 4 under "All Other Alloy Grades" and have been since SA 213-99.

 
Thank metengr,

I should've read the standard a little more closely. 'All other low alloy grades' was listed at the bottom of the low alloy steels section in table 4 of the ASTM A213 (2007) standard, along with the mechanical properties I was after.
 
I have tried to get them to move that line to the top of the table. Even knowing that it is there I have to hunt for it.

= = = = = = = = = = = = = = = = = = = =