Sep 5, 2006 #1 lahpe65 Structural Joined Jan 3, 2003 Messages 46 Location US I have found conflicting information regarding whether or not A194 Grade 2H can be galvanized. Can someone give me some guidance on this? Thanks in advance.
I have found conflicting information regarding whether or not A194 Grade 2H can be galvanized. Can someone give me some guidance on this? Thanks in advance.
Sep 5, 2006 #2 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US The guidance you need is referenced in ASTM A/SA-194. Please review this document, it references coatings and their limitations. Upvote 0 Downvote
The guidance you need is referenced in ASTM A/SA-194. Please review this document, it references coatings and their limitations.
Sep 5, 2006 Thread starter #3 lahpe65 Structural Joined Jan 3, 2003 Messages 46 Location US From what I read, A194 2H galvanized nut is a valid substitution for the A563 galvanized nut? Are there any loopholes I should be aware of? Upvote 0 Downvote
From what I read, A194 2H galvanized nut is a valid substitution for the A563 galvanized nut? Are there any loopholes I should be aware of?