Jul 19, 2004 #1 johnchrc Mechanical Joined Jul 14, 2004 Messages 176 Location US I am looking for the UTS of the subject material. I want to make a shear screw using 3/8-16 UNC and will turn the last 1/2" to size for shearing. I don't want to test this to determine the value. Does anyone have this information? Thanks.
I am looking for the UTS of the subject material. I want to make a shear screw using 3/8-16 UNC and will turn the last 1/2" to size for shearing. I don't want to test this to determine the value. Does anyone have this information? Thanks.
Jul 19, 2004 1 #2 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US The following properties are from the ASTM A 193 material specification; B7 material - 2.5" and under in diameter 125 Ksi min UTS, 105 Ksi min yield strength, 321 HB or 35 HRC max hardness Upvote 0 Downvote
The following properties are from the ASTM A 193 material specification; B7 material - 2.5" and under in diameter 125 Ksi min UTS, 105 Ksi min yield strength, 321 HB or 35 HRC max hardness