May 8, 2013 #1 jose0908 Petroleum Joined May 8, 2013 Messages 28 Location US We have some stainless steel Gate valves ASTM A182. Does ASTM A182 require for body and bonnet of valves to be stamped A182 on them?
We have some stainless steel Gate valves ASTM A182. Does ASTM A182 require for body and bonnet of valves to be stamped A182 on them?
May 10, 2013 2 #2 stanweld Materials Joined May 9, 2003 Messages 2,906 Location US Yes. Reference SA/A-961 section 20.1. Upvote 0 Downvote
May 16, 2013 Thread starter #3 jose0908 Petroleum Joined May 8, 2013 Messages 28 Location US Stanweld, Thanks for the advise Upvote 0 Downvote