Working for a tight company who wdon't like buying standards.

Can anyone let me know where I can get the Temperature and Pressure specification of ASTM A106 GrB pipe.

I am especially interested in the low temperature limits.

Regards,

Biggy
 
Replies continue below

Recommended for you

Low temp is -20 F unless you do charpy testing and then only down to -50 F.

If you work for a company too tight to buy a $33 standard then I doubt they would pay for the charpy testing.

Check B31.3 or B31.8 for the change in allowable stresses for higher temps.
 
team members

The Pressure and Temperature is listed on the approved Pining Classification Specification and all calculation support the Pressure and Temperature and components for the above material.
 