Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations JAE on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

ASTM A106 GrB. What is the Temp and Press range

Status
Not open for further replies.

Biggy

Mechanical
Joined
Feb 5, 2002
Messages
35
Location
NL
Working for a tight company who wdon't like buying standards.

Can anyone let me know where I can get the Temperature and Pressure specification of ASTM A106 GrB pipe.

I am especially interested in the low temperature limits.

Regards,

Biggy
 
Low temp is -20 F unless you do charpy testing and then only down to -50 F.

If you work for a company too tight to buy a $33 standard then I doubt they would pay for the charpy testing.

Check B31.3 or B31.8 for the change in allowable stresses for higher temps.
 
team members

The Pressure and Temperature is listed on the approved Pining Classification Specification and all calculation support the Pressure and Temperature and components for the above material.
 