Surveyor82
Industrial
I have a question about stress curves.
After doing some research I've found elaborate curves of A106 Gr.B in the API 530 about the rupture stresses but for the life of me, I can't find any data about A333 Gr.6. I don't think I can assume equivalence between the two since A333 Gr.6 is for preferred for low temperature service.
The problem is this: We have materials from both specs, only the first was required yet both are delivered. I want to know if A333 Gr.6 is capable of performing at elevated temperatures (> 400°C).
My preference is 'NO', but... I need sound information that it can or can't be used.
Any help would be amazing! Thanks in advance!
After doing some research I've found elaborate curves of A106 Gr.B in the API 530 about the rupture stresses but for the life of me, I can't find any data about A333 Gr.6. I don't think I can assume equivalence between the two since A333 Gr.6 is for preferred for low temperature service.
The problem is this: We have materials from both specs, only the first was required yet both are delivered. I want to know if A333 Gr.6 is capable of performing at elevated temperatures (> 400°C).
My preference is 'NO', but... I need sound information that it can or can't be used.
Any help would be amazing! Thanks in advance!