What is the difference between ASTM A105 and ASME SA105 ???

Thanks for you time
 
SA-105 and A-105 are the same material. ASME adds a "S" prefix to the ASTM materials they include in Section II.

Regards

Gunnar
 
Nukie,

Everything above is correct, however what is missing is the reason for the distinction.

ASME "SA" materials are permitted for use as components for ASME pressure vessels...... for example, one would expect to see SA105 carbon steel components on a vessel drawing.

ASTM "A" materials are permited for use in a Power or chemical process plant piping system designed to ASME B31.1 or B31.3.

Material Records must be maintained by the vessel fabicator for all "SA" materials......... the piping system fabricator must only supply evidence, in the form of a certificate of compliance, that the materials meet the "A" requirements.

Hope that this helps..............

MJC
 
MJCronin,

This is very interesting. I would like to know where this information is referenced. This could prove very useful in my job.

Lala
 