Asphalt durability in seawater

Status
Not open for further replies.

LittleWheels

Structural
Nov 27, 2001
358
I've been asked about topping a seaside boat ramp in AC. There are several aspects that concern me (eg friction and installation) but I'm also not sure about durability with seawater wetting/drying cycles. I vaguely recall a couple of tidal causeways in France that may be AC. Could somebody point me towards any research results on AC durability when cyclically exposed to seawater and UV?
 
Replies continue below

Recommended for you

DaveMinter - On the South Carolina coast many tidal region boat ramps are surfaced or totally constructed from asphalt - and last for decades. There is no problem with sea water. Here is a fact sheet from the Alabama Asphalt Pavement Association, see the very last paragraph

[idea]
 
Just for interest's sake, while on holidays in France I noted that the carparks at Mont St Michel are all below high tide level. A little care when visiting may be worthwhile!
 