Sep 29, 2011 #1 Elise Petroleum Joined Mar 21, 2002 Messages 10 Location US Does anybody know how I can EXTRAPOLATE Fig UCS-66 Curves upto 250mm thickness
Sep 29, 2011 #2 SectionIX Petroleum Joined Sep 19, 2011 Messages 283 Location US Extrapolation not necessary; final thickness notation at bottom of chart is >/= 75mm. Because it flatlines at 75mm, use that value as appropriate for your intended material/thickness.. Upvote 0 Downvote
Extrapolation not necessary; final thickness notation at bottom of chart is >/= 75mm. Because it flatlines at 75mm, use that value as appropriate for your intended material/thickness..
Sep 29, 2011 #3 SnTMan Mechanical Joined Jan 22, 2005 Messages 6,848 Location US Elise, perhaps you had better read UCS-66. Odd question for the forum. Regards, Mike Upvote 0 Downvote