Hi All,
We are supplying an ASME VIII Div 1 pressure vessel (wall thickness 15mm) containing process gas consisting of over 500ppm H2S. There is nothing in the clients specifications to state the vessel requires PWHT and they have not specified that the vessel is lethal service. After PO award and during discussions this week, the client has stated that the vessel requires PWHT.
As far as my limited knowledge of the code, PWHT is not required due to the thickness and according to para UW-2a, the vessel only requires PWHT if the end user has stated that the vessel is lethal service. Is the H2S quantity enough to automatically consider the vessel to be lethal service or does the client specifically need to state the vessel is lethal service? If they do need to state it, is there anywhere in the code this is written and also a definition of lethal service?
thanks,
Graeme
We are supplying an ASME VIII Div 1 pressure vessel (wall thickness 15mm) containing process gas consisting of over 500ppm H2S. There is nothing in the clients specifications to state the vessel requires PWHT and they have not specified that the vessel is lethal service. After PO award and during discussions this week, the client has stated that the vessel requires PWHT.
As far as my limited knowledge of the code, PWHT is not required due to the thickness and according to para UW-2a, the vessel only requires PWHT if the end user has stated that the vessel is lethal service. Is the H2S quantity enough to automatically consider the vessel to be lethal service or does the client specifically need to state the vessel is lethal service? If they do need to state it, is there anywhere in the code this is written and also a definition of lethal service?
thanks,
Graeme