Material SA-516Gr70, non-normalized, thickness=22.2 mm, design MDMT is -29°C
1. As per UG-20(f) it is exempted from impact test.
2. As per UCS-66, obtained -5°C of MDMT from curve B, so impact test required or use SA-516Gr70 normalized.
In view above, there is conflict between UG-20(f) and UCS-66 in some cases. This will make people confusing, which one we shall follow, UG-20(f) or UCS-66? This may virtually make a contradiction between the client/user and manufacturer. The manufacturer prefers UG-20(f), but client may prefer UCS-66.
1. As per UG-20(f) it is exempted from impact test.
2. As per UCS-66, obtained -5°C of MDMT from curve B, so impact test required or use SA-516Gr70 normalized.
In view above, there is conflict between UG-20(f) and UCS-66 in some cases. This will make people confusing, which one we shall follow, UG-20(f) or UCS-66? This may virtually make a contradiction between the client/user and manufacturer. The manufacturer prefers UG-20(f), but client may prefer UCS-66.